Vitrified tiles can't avoid the hollowing phenomenon? Paving

Vitrified tiles can't avoid the hollowing phenomenon? Paving

Time:2021-04-22 11:31:25 | Click:208

Because the surface of vitrified tiles is hard and smooth as a mirror, it has the advantages of practicability and beauty, so it is favored by many home improvement owners. However, the well-laid vitrified tiles cannot avoid the problems of hollowing and falling off, which has become a concern of the owners when decorating. In fact, there are many reasons for the hollowing and cracking of vitrified tiles. When paving construction, as long as you pay attention to methods and skills, you can effectively reduce the probability of this phenomenon.

QQ图片20200621112422.jpg

1. The paving environment is very important

The construction environment when laying vitrified tiles is very important, and the construction temperature should be between 5°C and 35°C. Because vitrified brick paving usually uses cement mortar as a binder, low temperature will reduce the hydration rate of cement, resulting in low early strength; and the water required for cement hydration will evaporate at high temperature, resulting in poor construction performance. Resulting in low final strength. At the same time, the working time of cement mortar is affected by temperature. The higher the temperature, the shorter the working time, the faster the cement setting, the earlier the mortar hardens, and the worse the water retention performance.

Of course, it is not recommended to lay vitrified tiles under strong winds. Because under strong winds, the moisture on the surface of the cement mortar will evaporate, which shortens the opening time and deteriorates the adhesive performance of vitrified tiles.In addition, if the mortar has hardened, no more water should be added. Because hardening is a precursor to the final setting of cement, adding water to stir the mortar also loses its workability.

QQ图片20200621112450.jpg

2. Stirring of the paste is very important

In order to make vitrified tiles paving firmly, it is very important to mix and stir the adhesive evenly. First of all, the material must be weighed in strict accordance with the instructions and requirements of the adhesive. Then, pour the liquid (water) component of the two-component into the mixing tank, and add half of the powder component to the mixing tank, and then stir at 300r/min, while stirring, add the remaining powder group Minute. After 1 minute, continue to stir at 200r/min for 3 minutes until there are no particles. Let it stand for 10 minutes. After the paste is fully cured, stir again for 3-5 minutes.

QQ图片20200621112508.jpg

3. the paving method is very important

The paving method of vitrified tiles is generally divided into two types: thick-layer back-pasting method and thin-layer construction method. The thickness of the thick layer backing method is about 15mm, which is easy to cause waste of tiles, and may increase the probability of cracking of the adhesive layer. It also makes a large cavity behind the tiles, which leads to the reduction of indoor space. In contrast, the thickness of the thin-layer construction method is only about 4mm, the back of the tiles is full and dense, and does not occupy the indoor space, the efficiency of paving is also higher, and the amount of tiles can also be saved.

In addition, you can also start with the basic treatment of the wall surface and the proper gaps.

How to choose a merchant for buying ceramic tiles online, an Understanding common misunderstandings in the quick start of